现在工程板房材料工程质量的需求不断的增加,在灾区临时我们需要通过使用的,而目前的市场的生产商厂家有大有小,难免有些信息技术及水平的不同而影响教学质量管理问题,那该如何提高辨别质量的呢?下面
济南工程板房厂家为您解答!
Now the demand for the engineering quality of engineering plank house materials is increasing, and we need to use them temporarily in the disaster area. However, there are many manufacturers in the current market, and it is inevitable that some differences in information technology and level will affect the teaching quality management. How can we improve the identification quality? Next, Jinan engineering plank house manufacturer will answer for you!
通过耳朵来判断,这个应该对很多材料都是可用的。我们用手指或者硬物敲击彩钢板,如果听到的声音是响亮且清脆的,那么材质肯定比较好。相反,如果发出来的声音听上去很闷,没有金属声音的话,那么这彩钢板的质量必然不好。
Judging by ear, this should be available for many materials. We hit the color steel plate with our fingers or hard objects. If the sound we hear is loud and clear, the material must be better. On the contrary, if the sound sounds dull and there is no metal sound, then the quality of the color steel plate must be poor.
仔细查看彩钢板外露钢材如断面等是否结晶细密,如果切面结晶细密,那么质量就是比较优良的。如果断面有发灰、发暗和杂质等,那么质量必然是不好的。
Carefully check whether the exposed steel of the color steel plate, such as the section, is finely crystallized. If the section is finely crystallized, the quality is relatively good. If the section has greying, darkening and impurities, the quality must be poor.
要从彩钢板内部的构造来检查了。彩钢板的主要构件有基板和彩色的腹膜或者镀层,基板和腹膜镀层的厚度达到一定的要求时,彩钢板的质量才会比较好。一般来说,比较好的彩钢板基板是0.02~0.05mm,覆膜或者涂层厚度往往只有0.15mm以下。
It is necessary to check from the internal structure of the color steel plate. The main components of the color steel plate are the base plate and the colored peritoneum or the coating. The quality of the color steel plate will be better when the thickness of the base plate and the peritoneum coating meets certain requirements. Generally speaking, the better color steel plate substrate is 0.02~0.05mm, and the film or coating thickness is usually only less than 0.15mm.
但是基板的厚度也是不可忽视的一点,因为它会影响防火活动房彩钢板的使用年限。一些生产彩钢板的厂家就会钻这个空子,在基板及彩钢板涂层或覆膜上做手脚。降低基板的厚度,但是增加了腹膜的厚度,表面看着似乎是质量很好。
However, the thickness of the base plate can not be ignored, because it will affect the service life of the color steel plate in the fireproof movable room. Some manufacturers of color steel plate will take advantage of this opportunity to do tricks on the substrate and color steel plate coating or film covering. The thickness of the substrate is reduced, but the thickness of the peritoneum is increased. It seems to be of good quality on the surface.
此外一间工程板房发生事故很不少,一些人被冰雹砸塌,一些人被火烧掉,住工程板房的人更需要注意,如果出现这种情况,立刻离开工程板房。建筑施工时被划分为两个主要因素,一是注意材料的优劣,二是注重建筑细节。更多相关内容就来我们网站
http://www.lxcaigang.com咨询吧!
In addition, there are many accidents in an engineering prefabricated house. Some people are collapsed by hail, and some people are burned down by fire. People living in engineering prefabricated houses need more attention. If this happens, leave the engineering prefabricated house immediately. Building construction is divided into two main factors, one is to pay attention to the quality of materials, and the other is to pay attention to architectural details. Come to our website for more relevant content http://www.lxcaigang.com Ask!